![](https://img66.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0d168420e79e215567a1d9095b27593aa29cd81d5c4a82ad45.jpg)
![](https://img66.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0dbc3a78b26cda8810bc68a6282ebb025f80382c31d04d524b.jpg)
![](https://img69.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0d2b1410ef491b49dc027a7097e5212302b1aea59fde710c8e.jpg)
![](https://img65.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0db0db68ed68ffa00b4b85a272e42b5ef8fdb56c2d0789bcea.jpg)
![](https://img65.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0d5bfedeb242a9b6d1acb9b31f0023f3cfab5f606296a48990.jpg)
![](https://img67.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0d17a3eb2558c04580625844dfa6573222047d5a9dcd3287fc.jpg)
![](https://img62.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0d404fa03a5e3742f937764ead5c88d8bd7129ae4f870eb54c.jpg)
![](https://img64.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0de43f1130f1c36686371800bbedf061c6f8e74bba721b133e.jpg)
![](https://img64.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0d15b8c92abf6a00355d06e7e53ab53ff4e21abdc0648e8fab.jpg)
![](https://img64.cn-america.cn/819f05fe9a3ee920c511d1a943f60d0d2c1c7dd772c88485e4363709ba97b1efb9d07fa2872c4fe8.jpg)
锈蚀钢板为什么要做锈面处理
1、迅速形成稳定的、颜色厚度均匀的、不容易被擦落的锈红色氧化膜,在室外温度摄氏25度的环境下,一般3小时内完成锈处理工艺。
2、锈处理催化方案下,迅速产生的表面粗糙有手感,使其构筑物更富体积感和质量感,升华视觉效果和感官效果,迅速提升园林设计的效果,提升经济效益和艺术效益!
一般锈钢板自然生锈要1-2年才有如此效果,2-3个月只有轻微黄锈色,没有手感,容易掉锈!
3、不受当地地理位置、当地天气、所位(面向东南还是西北)等影响,形成的锈红氧化膜颜色均匀一致稳定!
4、处理工艺不带腐蚀性,不会影响后期表面锈层的继续形成,环保无害,不影响植物的生长。不影响有限材料与周围植物的相互共生 ,体现可持续的设计观。